Eng
+1-480-493-0093

CeO2 deposeted by pulsing laser deposition on Ni-W

MDT-file: Download

CeO2_on_Ni-W
CeO2_on_Ni-W
Surface of CeO2 deposeted by pulsing laser deposition on Ni-W
 
Surface of CeO2 deposeted by pulsing laser deposition on Ni-W




size: 20x20 um
SPM principle: Intermittent contact mode